7075 aluminum rod, ultra-high strength aviation-grade aluminum alloy
7075 aluminum rod belongs to the Al-Zn-Mg-Cu series of super-hard aluminum alloys. After heat treatment strengthening, its strength is comparable to that of some steel materials. It is a core structural material in the aerospace and high-end equipment fields, combining ultra-high strength, good wear resistance, and fatigue resistance. It is known as the “strongest among aluminum alloys”.
Core performance advantages
Ultimate strength performance: In the T6 temper, the tensile strength can reach 540MPa, the yield strength is 480MPa, and the elongation is ≥11%. The strength far exceeds that of conventional aluminum alloys such as 6061;
Outstanding fatigue resistance and wear resistance: The addition of zinc, magnesium, and copper elements to the alloy composition forms a strengthening phase, making it less prone to deformation and wear under high-load conditions, resulting in a long service life;
Strong processing adaptability: capable of precision machining such as turning, milling, and drilling. After aging treatment in the T73 state, it can effectively reduce the risk of stress corrosion cracking, making it more suitable for harsh environments;
Significant lightweight characteristics: With a density of approximately 2.81g/cm³, it is only one-third of steel, offering clear advantages in scenarios where high strength and lightweight are pursued.
Mainstream specifications and status
Common tempers: T6 (peak strength state, suitable for high-strength demanding scenarios), T73 (corrosion resistance priority state, suitable for marine and humid environments), O (annealed soft state, easy for forming and processing);
Overall dimensions: round bars with diameters ranging from 5 to 300mm, square bars from 8 to 60mm, hexagonal bars with opposite sides ranging from 10 to 80mm. Lengths can be customized to 3m or 6m, and both fixed-length cutting and zero-cutting services are supported.
Typical application areas
Aerospace components, drone frames, high-end molds, sports equipment (hiking poles, bicycle frames), military equipment, core components of precision machinery, etc.
Core performance parameters of 7075 aluminum bar
Mechanical properties (under different heat treatment conditions)
| Condition | Tensile Strength (MPa) | Yield Strength (MPa) | Elongation (%) | Brinell Hardness (HB) |
| O (Annealed) | ≤276 | ≤145 | ≥17 | ≤60 |
| T6 (Peak Strength) | ≥540 | ≥480 | ≥11 | ≥150 |
| T73 (Corrosion-Resistant Aging) | ≥480 | ≥415 | ≥10 | ≥135 |
| T651 (Stress-Relieved) | ≥540 | ≥480 | ≥11 | ≥150 |
Physical properties
Density: 2.81g/cm³
Melting point: 475-635℃
Coefficient of thermal expansion (20-100℃): 23.6×10^-6/℃
Thermal conductivity (25℃): 130W/(m·K)
Electrical conductivity (20℃): 33% IACS
Elastic modulus: 71GPa
Poisson’s ratio: 0.33
Machinability
Machinability: Excellent. After cutting in the T6 temper, the surface finish is high, making it suitable for precision machining;
Formability: The formability is good in the O temper, but it becomes more difficult in the hardened state;
Heat treatment properties: Strengthening can be achieved through solution treatment + artificial aging. T6 is a commonly used peak strength treatment process, while T73 is an overaging treatment process, focusing on corrosion resistance.