Introduction of aluminum seamless tube 7075
7075 aluminum alloy is a high-strength aerospace-grade alloy, renowned as one of the strongest commercial aluminum alloys available.
Core Characteristics
Superior Strength
Its tensile strength reaches 500-570 MPa (after heat treatment), comparable to some low-carbon steels, making it ideal for high-load applications.
Excellent Mechanical Properties
It offers good fatigue resistance and moderate toughness, balancing strength and usability.
Heat-Treatable
It can be strengthened through T6, T651, or T73 heat treatment processes to optimize performance for specific needs.
Corrosion Performance
While naturally less corrosion-resistant than 5xxx or 6xxx series alloys, it can be protected via anodizing, painting, or clad layers (e.g., 7075-T6 clad sheets).
Key Alloy Composition
The primary alloying elements are zinc (5.1-6.1%), magnesium (2.1-2.9%), and copper (1.2-2.0%), with small additions of chromium (0.18-0.28%) to enhance grain structure and corrosion resistance.
Typical Applications
Aerospace: Aircraft fuselages, wings, landing gear components, and structural parts due to its high strength-to-weight ratio.
Industrial Machinery: High-load parts like gears, shafts, and tooling fixtures.
Automotive: Performance vehicle components (e.g., suspension parts) and racing car structures.
Marine: Boat hulls and deck fittings (when corrosion protection is applied).
Sports Equipment: Bicycle frames, climbing gear, and high-end golf club heads.
Processing Notes
It can be machined, welded (with proper techniques to avoid cracking), and formed (though formability is lower than softer aluminum alloys).
Welding requires matching fillers (e.g., ER5356) and pre/post-heat treatments to maintain integrity.
Technical Parameters
Based on GB/T 4437.1-2023 (Aluminium and aluminium alloys extruded seamless tubes — Part 1: Seamless round tubes) and its normative reference GB/T 3190 (which defines the chemical composition), here is the requested data for 7075 Aluminium Alloy Hot-Extruded Seamless Tube:
1. Chemical Composition — 7075 (per GB/T 3190, referenced by GB/T 4437.1-2023)
| Element | Symbol | Content (%) |
|---|---|---|
| Silicon | Si | ≤ 0.40 |
| Iron | Fe | ≤ 0.50 |
| Copper | Cu | 1.20 – 2.00 |
| Manganese | Mn | ≤ 0.30 |
| Magnesium | Mg | 2.10 – 2.90 |
| Chromium | Cr | 0.18 – 0.28 |
| Zinc | Zn | 5.10 – 6.10 |
| Titanium | Ti | ≤ 0.20 |
| Others (each) | — | ≤ 0.05 |
| Others (total) | — | ≤ 0.15 |
| Aluminum | Al | Remainder |
2. Room-Temperature Tensile Mechanical Properties — 7075 Seamless Extruded Tube (per Table 3 of GB/T 4437.1-2023)
Wall thickness in mm, Rm = Tensile Strength, Rp0.2 = Proof Strength, A = Elongation (min).
7075 — T6 / T6510 / T6511 Condition
| Wall Thickness (mm) | Rm (MPa) min | Rp0.2 (MPa) min | Elongation A (min) |
|---|---|---|---|
| ≤ 6.30 | 540 | 480 | — |
| > 6.30 – 12.50 | 560 | 505 | — |
| > 12.50 – 70.00 | 560 | 505 | — |
(A₅₀ₘₘ elongation applies where specified; for tube wall, A (original gauge length proportional to √S₀) is used per standard.)
7075 — T73 / T73510 / T73511 Condition
| Wall Thickness (mm) | Rm (MPa) min | Rp0.2 (MPa) min | Elongation A (min) |
|---|---|---|---|
| 3.50 – 6.30 | 470 | 400 | — |
| > 6.30 – 35.00 | 485 | 420 | — |
| > 35.00 – 70.00 | 475 | 410 | — |
7075 — O Condition
| Wall Thickness (mm) | Rm (MPa) max | Rp0.2 — | Elongation A (min) |
|---|---|---|---|
| ≤ 10.00 | ≤ 275 | — | — |
3. Dimensional Tolerances (Outside Diameter & Wall Thickness)
Per GB/T 4437.1-2023Clause 5 & Table 2, dimensions and allowable deviations shall comply with GB/T 4436 Aluminium and aluminium alloys — Tubes — Dimensions and tolerances.
- Maximum outside diameter of seamless tube: ≤ 580 mm
- Tolerance class: if not specified in order → supplied as Normal Grade
- OD and wall thickness tolerance grades (High Precision / Normal / Rough) are defined in GB/T 4436 based on nominal size.
Typical (Normal Grade) example from GB/T 4436:
| Nominal OD (mm) | OD Tolerance (± mm) | Wall Thickness Tolerance (± mm) |
|---|---|---|
| ≤ 25 | ±0.30 | ±0.35 |
| > 25 – 50 | ±0.45 | ±0.50 |
| > 50 – 100 | ±0.70 | ±0.75 |
| > 100 – 200 | ±1.10 | ±1.10 |
(Exact values depend on specified tolerance class per GB/T 4436— user / purchaser may designate precision grade in order.)