7A55 Ultra-High-Strength Aluminum Alloy: Technical Datasheet for Aerospace & Defense
1. Material Overview
7A55 is a high-purity, Zr-modified Al–Zn–Mg–Cu alloy developed to meet the most demanding structural requirements in aviation, armored systems, and advanced manufacturing. It is recognized domestically and internationally as a direct replacement and upgrade for 7055 and 7050 alloys, with improved strength-toughness balance, thicker-section capability, and better environmental durability.

Core Advantages
- Tensile Strength: 600–650 MPa
- Yield Strength: 570–620 MPa
- Fracture Toughness (KIC): 35–42 MPa·√m (significantly higher than 7055)
- Hardenable Thickness: Up to 160 mm+
- Low-Temperature Stability: No brittle fracture at –50°C
- Stress Corrosion Resistance: Excellent, suitable for marine deployment
- Weld Joint Efficiency: 55–65% (with ER5356/ER5556 wire)
Standards Compliance
GJB 2662A, GB/T 3880, AMS 4206, AMS 4336, EN 573-3, ASTM B594, ASTM E112
2. Product Forms & Applications by Thickness
| Thickness Range | Product Form | Recommended Tempers | Typical Applications |
|---|---|---|---|
| 0.2–2.0 mm | Sheet / Strip | T6, T651, T7651 | Aircraft skin, light ballistic plates, thin-walled structural parts |
| 2.0–6.0 mm | Rolled Plate | T6, T651, T7651 | Fuselage panels, helicopter structures, light armor facings |
| 6–25 mm | Medium Plate | T6, T651, T7751 | Secondary aircraft structures, side armor, bulkheads |
| 25–100 mm | Heavy Plate | T651, T7751, T7951 | Wing spars, landing gear, heavy armor, main frames |
| 100–150 mm | Extra-Heavy Plate | T7751, T7651, T652 | Large forgings, heavy ballistic plate, tank hulls |
| 150–300 mm | Forgings / Thick Plate | T7751, T652 | Aircraft primary forgings, 12.7 mm ballistic protection, heavy-duty molds |
Key Sectors: Civil and military aircraft (including C919), rotorcraft wheels, armored fighting vehicles, naval decking, spacecraft structures, precision tooling, and ballistic shielding.
3. Chemical Composition (wt%)
| Element | Si | Fe | Cu | Mn | Mg | Cr | Zn | Ti | Zr | Others (Each) | Others (Total) | Al |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Limit | ≤0.10 | ≤0.12 | 2.0–2.6 | ≤0.20 | 1.8–2.5 | ≤0.04 | 7.8–8.8 | ≤0.06 | 0.10–0.25 | ≤0.05 | ≤0.15 | Bal. |
Design Features:
- Ultra-high Zn for maximum strength
- Zr for fine grain size, toughness, and thick-section hardenability
- Minimal Fe/Si for improved fracture resistance
- Elevated Cu for thermal stability, fatigue life, and weldability
4. Mechanical Properties by Temper
| Temper | Tensile Strength (MPa) | Yield Strength (MPa) | Elongation A₅₀ (%) | Hardness (HBW) | Stress Corrosion | Positioning |
|---|---|---|---|---|---|---|
| T6 | 580–650 | 540–610 | 6–9 | 158–170 | Moderate | Peak strength |
| T651 | 560–630 | 520–590 | 7–10 | 155–165 | Moderate | Stress-relieved plate |
| T7651 | 550–600 | 510–570 | 8–11 | 152–162 | Good | Balanced strength & corrosion |
| T7751 | 600–650 | 570–620 | 8–12 | 158–168 | Excellent | Flagship aerospace/armor |
| T7951 | 570–620 | 540–590 | 9–12 | 153–163 | Good | Fatigue/toughness priority |
Typical Toughness Range: 28–45 MPa·√m depending on temper and thickness
Fatigue Strength: 150–195 MPa (10⁷ cycles, R=0.1)
5. Physical Properties
- Density: 2.82 g/cm³
- Elastic Modulus: 71 GPa
- Melting Range: 475–655°C
- Thermal Conductivity: 130–150 W/m·K
- Electrical Conductivity: 22–27% IACS
- CTE: 23.6 μm/m·°C
- Poisson’s Ratio: 0.33
6. Heat Treatment & Processing
Solution Treatment: 465–476°C, water quench
Aging Options:
- T6: 120–140°C / 20–24 h (peak strength)
- T7751: 120°C → 175–185°C → 125°C (optimal all-round performance)
- T7951: T6 + 170–180°C secondary aging (fatigue/toughness focus)Stress Relief: ≥1.5–3% pre-stretch for plates >25 mm
Machining: Excellent finish with carbide tooling + high coolant flow
Welding: MIG/TIG with ER5356/ER5556; FSW yields higher joint efficiency (up to ~65%)
Forming: Thin sheet allows mild cold bending; heavy sections require hot forming or machining
7. Ballistic Performance (STANAG 4569 / NIJ)
| Threat Level | Plate Thickness Required |
|---|---|
| NIJ II | 5–7 mm |
| NIJ IIIA | 7–9 mm |
| STANAG Level 1 | 9–11 mm |
| STANAG Level 2 | 12–16 mm |
| STANAG Level 3 (12.7 mm AP) | 22–28 mm |
Compared to 7039-T73, 7A55 achieves equivalent protection at 3–5 mm less thickness, significantly reducing system weight.
8. Ultrasonic Testing Acceptance (AMS-STD-2154 / ASTM B594)
| Thickness | Max Allowable Defect (Flat-Bottom Hole Equivalent) |
|---|---|
| ≤12.5 mm | ≤Φ1.2 mm |
| 12.5–100 mm | ≤Φ1.6 mm |
| 100–300 mm | ≤Φ2.0 mm |
Rejection criteria include lamination, cracks, clustered inclusions, or excessive back-wall echo attenuation.
9. Selection Guide
| Requirement | Recommended Temper |
|---|---|
| Aerospace primary structure | T7751 |
| Heavy armor / 12.7 mm protection | T7751 |
| Low-temperature service (–50°C) | T7751 |
| Welded assemblies | T7751 |
| Cost-sensitive light structures | 7039-T73 |