7A52 Aluminum Alloy: China’s 2nd Gen Military Armor Plate (GJB 1540)
- Material Overview
7A52 is a heat‑treatable, high‑strength Al–Zn–Mg wrought aluminum alloy (formerly LC52). Developed as China’s second‑generation armor aluminum alloy, it is standardized under GJB 1540 and widely used in military equipment such as combat vehicle components and turrets. It is the only military‑grade weldable high‑strength aluminum alloy, offering an optimal balance of strength, weldability, and cost‑effectiveness.
Core Advantages
- Superior weldability: Best‑in‑class among 7000‑series alloys; compatible with MIG and FSW
- High strength: Tensile strength 469–600 MPa, yield strength 424–520 MPa
- Lightweight: Density ~1/3 of steel; 6–20 % weight reduction for armor
- Low‑cycle fatigue resistance: Excellent for dynamic military loads
- Cost‑effective: Lower cost than aerospace 7050/7055; mass‑production ready
Standards Compliance
- GJB 1540: Military armor aluminum specification
- GB/T 3880: Wrought aluminum chemical composition
- GB/T 228.1: Mechanical testing
- Chemical Composition (Mass Fraction, %)
| Element | Zn | Mg | Cr | Zr | Cu | Fe | Si | Others (Ind.) | Others (Total) | Al |
| Limit | 4.0–4.8 | 2.0–2.8 | 0.15–0.25 | 0.05–0.15 | 0.05–0.20 | ≤0.30 | ≤0.30 | ≤0.05 | ≤0.15 | Balance |
Key Notes
- Zn/Mg: Main strengthening elements; form MgZn₂ precipitates
- Cr/Zr: Grain refiners; enhance toughness and weldability
- Low Cu: Improves weldability; avoids hot cracking
- Military grade: Precise trace element tuning for performance
III. Mechanical Properties (Full Thickness / Multi‑Temper)
Typical Properties by Temper
| Temper | Thickness | Tensile Strength (MPa) | Yield Strength (MPa) | Elongation (%) | Hardness (HB) | Typical Application |
| T4 | 0.1–300 mm | 345–450 | 275–350 | 12–18 | 90–110 | Formable, low‑load components |
| T6 | 0.1–300 mm | 469–600 | 424–520 | 9–14 | 130–150 | Armor, gun mounts, core structures |
| T651 | 6–300 mm | 450–580 | 400–500 | 8–13 | 125–145 | Large armor plates, forgings |
| H112 | 10–300 mm | 380–480 | 290–380 | 10–16 | 100–120 | As‑hot‑worked forgings |
Key Notes
- Thin plates (≤1 mm): T6 strength 469–550 MPa, elongation ≥10 %
- Extra‑thick (>100 mm): T6 strength ≥450 MPa
- Impact toughness: ≥25 J/cm² (military requirement)
- Heat Treatment Specifications
- Homogenization
- 460 ±10 °C / 20–24 h, slow cool to 200 °C then air cool
- Purpose: Eliminate segregation, refine grains
- Solution Treatment
- 470 ±5 °C, hold by thickness
- 1–6 mm: 30–60 min
- 6–100 mm: 60–120 min
- 100–300 mm: 120–180 min
- Water quench (20–40 °C), cooling rate ≥150 °C/h
- Aging
- T4: Natural aging ≥96 h
- T6: 120 ±5 °C / 24 h
- T651: 1.5–3 % tension relief + T6 aging
- Post‑Weld Aging
- 120 °C / 12–24 h; restores ≥70 % base strength
- Processing Characteristics
Rolling
- Thin (0.1–6 mm): Cold roll, 10–15 % pass reduction
- Medium (6–100 mm): Hot roll 400–450 °C, ≥350 °C finish
- Thick (>100 mm): Hot roll/forging combo, UT required
Forging
- Preheat 400–450 °C, hold 2–4 h
- Forging ratio 3–5, finish ≥350 °C
Machining
- T6: Carbide tools, 80–120 m/min, 0.1–0.2 mm/r
Surface Treatment
- Anodizing, military paint, or Al‑clad for corrosion resistance
- Welding Performance
Welding Methods
- MIG: 3–20 mm, ER5356/5A56/5B06
- FSW: 3–50 mm, no filler
- Double‑wire MIG: 5–30 mm
- Electron beam: 10–50 mm
Weld Strength
- Joint strength ≥70 % base metal; typical 275 MPa
Material Selection Guide
| Alloy | Weldability | Tensile Strength | Primary Use |
| 7A52 | Good | 469–600 MPa | Armor, welded structures |
| 7022 | Poor | 560–620 MPa | Aviation components |
| 7050 | Poor | 560–580 MPa | Aerospace structures |
| 7055 | Very poor | 580–650 MPa | Ultra‑high‑strength parts |
Conclusion: Choose 7A52 for welded armor/gun mounts.
VII. Ultrasonic Testing (UT)
Standards
- Military: GJB 1580
- Industrial: ASTM B594/B548
Acceptance Defects
| Thickness | Military Grade | Industrial Grade |
| ≤12.5 mm | ≤Φ1.2 mm | ≤Φ1.6 mm |
| 12.5–100 mm | ≤Φ1.6 mm | ≤Φ2.0 mm |
| 100–300 mm | ≤Φ2.0 mm | ≤Φ2.5 mm |
Rejection Criteria
- Delamination, cracks, dense inclusions, porosity
VIII. Grain Size (ASTM E112 / GB/T 3246.1)
| Product | Thickness | Grade | Avg Size |
| Thin sheet | 0.2–6 mm | ≥7 | ≤20 μm |
| Medium plate | 6–100 mm | ≥6 | ≤30 μm |
| Thick plate | 100–300 mm | ≥5 | 30–50 μm |
- Dimensional Tolerances
| Thickness | GB/T 3880 | EN 485‑4 | ASTM B209 |
| 0.2–0.6 mm | ±0.03 | ±0.03 | ±0.03 |
| 0.6–2.0 mm | ±0.10 | ±0.10 | ±0.10 |
| 2.0–6.0 mm | ±0.25 | ±0.25 | ±0.25 |
| 6.0–25 mm | ±0.60 | ±0.60 | ±0.60 |
| 25–100 mm | +1.0/0 | +1.0/0 | +0.8/0 |
| 100–200 mm | +1.2/0 | +1.2/0 | +1.0/0 |
| 200–300 mm | +1.5/0 | +1.5/0 | +1.2/0 |
- Production Process
T6
Melting → degassing → homogenization → rolling/forging → solution → aging → finishing → UT
T651
Homogenization → rolling → solution → tension relief → aging → finishing
T4
Homogenization → rolling → solution → natural aging → finishing
H112
Forging → air cool → finishing → UT


Leave a Reply