7075-T7351 vs T651: Solving Stress Corrosion & Machining Deformation
1. Material Overview: Why 7075T7351/T7352 Stands Out
7075T7351/T7352 is a premium AlZnMgCu series ultra-high strength aluminum alloy in the over-aged stress-relieved condition—engineered to balance performance and durability for demanding environments. Its core advantage: sacrificing only 10-15% of tensile strength (vs. T651) to deliver 2-3x better stress corrosion cracking (SCC) resistance, superior toughness, and zero deformation during processing.
1.1 Key Specifications
Thickness Range: 6.3-100mm (T7351); 100-300mm (T7352, compression stress relief for minimal residual stress).
Production Process: Solution heat treatment → rapid water quenching → 1.5%-3% stretch/compression stress relief → over-aging (T73) → straightening → finishing.
Core Benefits:
Highest-level SCC & exfoliation corrosion (EXCO) resistance
Extremely low residual stress & dimensional stability
Traceable mechanical properties & alloy composition
Recyclable & energy-efficient (aligns with sustainability goals)
1.2 Industrial Applications
Aviation primary load-bearing structures, shipborne equipment, precision molds, marine engineering, offshore oil platforms, high-reliability components for long-term service—where corrosion resistance and structural integrity are non-negotiable.
2. Alloy Composition (Mass Fraction %)
Compliant with EN 573-3 / ASTM B209 / AMS 4078, guaranteeing consistency and compatibility with global manufacturing standards.
|
Element |
Si | Fe | Cu | Mn | Mg | Cr | Zn | Ti | Other (Single) | Other (Total) | Al |
| Standard Value | ≤0.40 | ≤0.50 | 1.2~2.0 | ≤0.30 | 2.1~2.9 | 0.18~0.28 | 5.1~6.1 | ≤0.20 | ≤0.05 | ≤0.15 | Remainder |
2.1 Core Element Functions (Critical for Performance)
Zn: Forms MgZn₂ strengthening phase, delivers primary tensile strength
Mg: Synergizes with Zn for stability in over-aged microstructures
Cu: Enhances strength, improves SCC resistance, and refines grain structure
Cr: Inhibits recrystallization, boosts toughness, and reinforces corrosion resistance
3.Thickness Segmentation & Condition Definition
3.1 Thickness Intervals (Tailored for Optimal Performance)
6.3-100mm: 7075T7351 (stretch stress relief + over-aging) – standard for most industrial uses.
100-300mm: 7075T7352 (compression stress relief + over-aging) – ideal for extra-thick plates requiring minimal residual stress.
3.2 T73 Over-Aging Advantage
The T73 process moderately coarsens strengthening phases and eliminates continuous grain boundary precipitates—completely solving stress corrosion issues that plague less advanced tempers.
4.Mechanical Properties (Tested & Verified)
4.1 7075T7351 (6.3-100mm)
|
Thickness (mm) |
Tensile Strength (MPa) | Yield Strength (MPa) | Elongation (%) (A50mm) | Hardness (HBW) |
|
6.3-12.5 |
≥470 | ≥385 | ≥7 |
125-135 |
|
12.5-25 |
≥470 | ≥385 | ≥6 |
125-135 |
|
25-50 |
≥460 | ≥370 | ≥5 |
125-135 |
| 50-100 | ≥450 | ≥360 | ≥5 |
125-135 |
4.2 7075T7352 (100-300mm) – Source: ASTM B247M / AMS 4078
|
Thickness (mm) |
Tensile Strength (MPa) | Yield Strength (MPa) | Elongation (%) |
|
100-150(T7351) |
≥450 | ≥360 | ≥5 |
| 150-200(T7352) | ≥440 | ≥350 |
≥5 |
| 200-300(T7352) | ≥430 | ≥340 |
≥5 |
5. Critical Comparison: 7075T7351 vs. T651 (User’s Key Decision Point)
| Performance Metric | T651 (Peak Aging) | T7351 (Over-Aging) |
| Tensile Strength | High | 10%~15% Lower |
| Yield Strength | High | 10%~15% Lower |
| Stress Corrosion Cracking (SCC) Resistance | Moderate | Excellent (Meets aviation’s highest standards) |
| Fracture Toughness | Medium | Higher |
| Residual Stress | Low | Extremely Low |
| Processing Deformation | Minor | Minimal |
| Electrical Conductivity | ~33% IACS | ~40% IACS (Rapid over-aging verification) |
When to Choose T7351/T7352: For applications requiring long service life, exposure to corrosive environment (e.g., marine, offshore), or precision machining with zero deformation.
6. Dimensional Tolerances (Multiple Standards Supported)
6.1 6.3-100mm (T7351)
|
Dimension (mm) |
EN 485-4 Group II | US Standard (General) | US Standard (Aviation) |
| TH: 6.3-10 | +0.30 | +0.25 |
+0.20 |
|
TH: 10-25 |
+0.40 | +0.30 | +0.25 |
|
TH: 25-50 |
+0.50 | +0.40 | +0.30 |
| TH: 50-100 | +0.80 | +0.60 |
+0.45 |
| Width≤1250 | +4 | +3.2 |
+1.6 |
| Length≤3000 | +6 | +3.2-+6.4 |
+1.6-+3.2 |
6.2 100-300mm (T7352)
|
Thickness (mm) |
EN 485-4 Group II | US Standard (General) | US Standard (Aviation) |
|
100-150 |
+1.0 | +0.8 | +0.6 |
| 150-300 | +1.2 | +1.0 |
+0.7 |
7. Quality Control: Ultrasonic Testing (UT) – ASTM B594
Aviation Grade: 100-150mm ≤Φ1.6mm; 150-300mm ≤Φ2.0mm
General Grade: 100-150mm ≤Φ2.0mm; 150-300mm ≤Φ2.5mm
Rejection Criteria: Cracks, shrinkage cavities, dense inclusions; bottom wave loss >80%
8. Grain Size (ASTM E112)
T7351 (6.3-100mm): ≥Grade 6, ≤25μm (fine grain for superior toughness)
T7352 (100-300mm): ≥Grade 5, 25-50μm (optimized for thick-plate stability)
9. Production Process (Transparent & Traceable)
Melting & casting → Homogenization annealing → Hot rolling to target thickness
Solution heat treatment + rapid water quenching (critical for strength retention)
Stretch/compression stress relief (1.5%-3%)
Over-aging heat treatment (core of T73 technology)
Leveling → Precision cutting → UT inspection → Mechanical performance testing → Warehousing.
10. Key Takeaways for Engineers & Buyers
Standard Compliance: All data traceable to ASTM B209/AMS 4078/EN 573-3- no fabricated specifications.
Corrosion Resistance Priority: The #1 choice for long-service-life components in corrosive environments.
Thickness Matters: >100mm requires T7352 for minimal residual stress and dimensional stability.
Sustainability: Fully recyclable, aligning with global industrial sustainability objectives.
For custom thicknesses, specifications, or application-specific technical support, contact our engineering team.
Alex Xu
Sales Engineer
Tel: +8615261610498
Email: info@newalatomic.com


Leave a Reply