7075 Aluminum Sheet (0.5–4.0 mm): Aerospace‑Grade Technical Datasheet
Product Introduction
7075 is an Al‑Zn‑Mg‑Cu alloy often called the “King of Aluminum Alloys.” Its unique chemistry and heat treatment response make it the go‑to material when projects demand extreme strength, high fatigue resistance, and low weight.

Core Benefits
- Tensile Strength: 540–550 MPa (T6/T651)
- Yield Strength: 460–480 MPa (T6/T651)
- Density: 2.81 g/cm³
- Fully compliant with ASTM B209, AMS 4049, EN 573‑3 / EN AW‑7075
Common Trade‑Offs
- Moderate corrosion resistance (use cladding or coatings for harsh environments)
- Poor weldability (mechanical fastening or bonding recommended)
- Requires controlled heat treatment to avoid stress corrosion cracking
Chemical Composition (wt%)
| Element | Si | Fe | Cu | Mn | Mg | Cr | Zn | Ti | Others (Single) | Others (Total) | Al |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Range | ≤0.40 | ≤0.50 | 1.2–2.0 | ≤0.30 | 2.1–2.9 | 0.18–0.28 | 5.1–6.1 | ≤0.20 | ≤0.05 | ≤0.15 | Bal. |
Key Strengthening Mechanism: Zn and Mg form MgZn₂ precipitates; Cu enhances strength, toughness, and corrosion performance; Cr refines grain structure.
Available Tempers & Mechanical Properties
7075‑O (Annealed)
Best for deep drawing or forming before final heat treatment.
| Thickness (mm) | Tensile Strength (MPa) | Yield Strength (MPa) | Elongation (%) |
|---|---|---|---|
| ≤1.5 | 220–260 | ≤100 | ≥16 |
| 1.5–3.0 | 220–260 | ≤100 | ≥15 |
| 3.0–4.0 | 220–260 | ≤100 | ≥14 |
7075‑T6 (Peak Strength)
Maximum hardness and strength for structural parts.
| Thickness (mm) | Tensile Strength (MPa) | Yield Strength (MPa) | Elongation (%) |
|---|---|---|---|
| 0.8–1.5 | ≥540 | ≥460 | ≥6 |
| 1.5–3.0 | ≥540 | ≥470 | ≥7 |
| 3.0–4.0 | ≥545 | ≥475 | ≥8 |
7075‑T651 (Stress Relieved)
T6 plus stretching to reduce machining distortion—preferred for precision aerospace parts.
| Thickness (mm) | Tensile Strength (MPa) | Yield Strength (MPa) | Elongation (%) |
|---|---|---|---|
| 0.8–1.5 | ≥540 | ≥460 | ≥6 |
| 1.5–3.0 | ≥540 | ≥470 | ≥7 |
| 3.0–4.0 | ≥545 | ≥475 | ≥8 |
Dimensional Tolerances (0.5–4.0 mm)
| Standard | Thickness Tolerance | Width/Length Tolerance |
|---|---|---|
| EN 485‑1 / 485‑4 (Group II) | ±0.05 mm (≤2.0 mm) ±0.10 mm (2.0–4.0 mm) |
+0.06/–0.04 mm (≤1.0 mm) +0.07/–0.05 mm (1.1–2.0 mm) +0.08/–0.06 mm (2.1–3.0 mm) +0.10/–0.08 mm (3.1–4.0 mm) |
| ANSI H35.2 (Commercial) | ±0.0015–0.0035 in | +3.2–6.4 mm |
| ANSI H35.2 (Aerospace) | Tighter than commercial | +1.6–3.2 mm |
Surface Quality: Processed in an air cushion furnace—no roller marks, scratches, or handling defects.
Manufacturing Workflow
7075‑O (0.5–4.0 mm)
- Casting & homogenization
- Hot rolling to intermediate thickness
- Cold rolling to final gauge
- Annealing for maximum formability
- Leveling, cutting, inspection
7075‑T6/T651 (0.5–4.0 mm)
- Casting → hot rolling → cold rolling
- Solution heat treatment + rapid water quench
- Artificial aging (T6)
- Stretching for stress relief (T651 only)
- Final finishing and QA release
Applications
- Aerospace: Wing skins, fuselage panels, door frames, precision brackets
- Motorsports: Chassis parts, suspension arms, roll cages
- Industrial Tooling: Injection molds, robotic arms, precision jigs
- Defense: Lightweight armor substrates, structural supports
Selection Guide
| Requirement | Recommended Temper |
|---|---|
| Forming before heat treatment | 7075‑O |
| Maximum strength, minimal machining | 7075‑T6 |
| Precision machining, flatness critical | 7075‑T651 |