5083 aluminum is widely used in marine, automotive, pressure vessels, and structural applications. However, 5083-O and 5083-H111 are not interchangeable, especially when forming or bending is involved.

Property 5083-O (Annealed) 5083-H111 (Lightly Work-Hardened)
Tensile Strength (MPa) 275–310 290–330
Yield Strength (MPa) 125–145 145–185
Elongation A₅₀ (%) 22–28 16–22
Uniform Elongation Ag (%) 18–22 12–16
Hardness (HBW) 60–70 70–80

Although tensile strength overlaps, 5083-H111 has about 25% lower ductility, making it unsuitable for deep drawing or tight-radius bending.

Why does 5083-O have better formability than H111?

The key lies in microstructure and strain behavior:

  • 5083-O: Fully annealed, equiaxed grains, very low dislocation density → excellent plasticity.
  • 5083-H111: Light cold work (~≤5%) introduces dislocations → higher yield strength but reduced stretchability.

In practical forming tests:

  • Flanging capability: 5083-O achieves a flanging coefficient of 0.65, while H111 fails at 0.80.
  • Bending radius: O-temper bends safely at 1t radius; H111 requires ≥2.5t​ to avoid cracking.

When should I use 5083-O aluminum?

Choose 5083-O​ when your application involves:

✅ Deep drawing

✅ Complex flanging

✅ Bending radius < 2t​

✅ Marine structures requiring maximum corrosion resistance

✅ Pressure vessels with high stress stability requirements

5083-O is the safest choice for any process where plastic deformation is significant.

When is 5083-H111 acceptable?

5083-H111​ is suitable for:

✅ Structural frames and supports

✅ Non-forming sheet metal parts

✅ CNC machining panels

✅ Decorative or surface-critical applications without bending

It offers higher yield strength and lower material cost but must not be used for large deformation processes.

Is 5083-H111 cheaper than 5083-O?

Yes—5083-H111 typically costs about 15% less​ due to simpler processing.

However, using H111 in forming applications often leads to:

❌ Cracking during production

❌ High scrap and rework rates

❌ Delivery delays and financial penalties

In many cases, the total cost exceeds the savings from choosing O-temper.

What tests should be done before production?

For any part involving forming, we recommend verifying:

  1. Work hardening exponent (n-value)​ > 0.28
  2. Plastic strain ratio (r-value)​ > 0.9 for O-temper
  3. Simulated bend test​ at the minimum design radius

Do not rely on tensile strength alone—ductility determines success.

Can 5083-H111 replace 5083-O in my project?

No.​

5083-O can cover all applications suitable for H111, but H111 cannot replace O-temper in forming-heavy designs.

If your component requires:

  • Local thinning > 15%
  • Bending radius < 2t
  • Flanging or deep drawing

→ Always specify 5083-O.

Need help selecting the right 5083 aluminum temper?

We supply both 5083-O and 5083-H111 aluminum plates, bars, and forgings, with full mechanical test reports and EN 10204 3.1 certificates.

Contact our technical team for:

  • Material selection advice
  • Formability risk assessment
  • Custom cutting and export packaging

Frequently Asked Questions (FAQ)

Q: Is 5083-O softer than H111?​

A: Yes. It has lower hardness and yield strength, which allows greater deformation without cracking.

Q: Will H111 crack if I bend it?​

A: Only at larger bend radii (≥2.5t). Small-radius bends will likely cause edge cracking.

Q: Which temper is best for marine use?​

A: 5083-O is preferred for welded marine structures due to superior corrosion resistance and stress stability.