sample of 5083H131 aluminum sheet with Inkjet coding

5083 H321 vs H131 Aluminum Plate – Process & Performance Comparison(Revision)

  1. Revision Notes

This revised document addresses five critical issues in the original version: confused standard systems, incorrect process parameters, inaccurate mechanical data, misused terminology, and logical inconsistencies. It clearly separates the applicable standards for H321 and H131, corrects stabilization temperature/time, strain hardening levels, mechanical properties, and standard terms, ensuring full compliance with international specifications and eliminating misleading information.

  1. Key Corrected Issues
  2. Standard System Confusion

Removed mixed use of EN/ASTM/MIL standards.

  • 5083 H321: EN 485, ASTM B209/B928
  • 5083 H131: ASTM B209/B928, MIL-DTL-46027K
  • Note: H131 is not defined in EN 485-2.
  1. Incorrect Process Parameters
  • Stabilization temperature: 120°C – 175°C for both tempers
  • Stabilization time:
    • H321: 1–2 hours (typical thickness)
    • H131: 3–5 hours (longer for thick plates)

Removed invalid “h/mm” time unit; replaced with standard stabilization terms.

  1. Mechanical Property Deviations
  • H321 tensile strength: 305–350 MPa (thin plate)
  • H131 yield strength: ≥240 MPa
  • Strength difference adjusted to 10%–15% per standard requirements.
  1. Incorrect Strain Hardening Ranges
  • H321: 15%–25%
  • H131: 20%–35%

Consistent with H131 as the higher-strength temper.

  1. Misused Terminology
  • “Softening temperature” → Stabilization temperature
  • “Softening time” → Stabilization holding time
  • “Cold work rate” → Strain hardening level (cold work degree)
  1. 5083 H321 vs H131 – Process & Performance Table (Revised)
Item 5083‑H321 5083‑H131
Applicable Standards EN 485, ASTM B209/B928 ASTM B209/B928, MIL‑DTL‑46027K
Process Route Cold work (15%–25%) + low‑temperature stabilization Higher cold work (20%–35%) + stabilization + stress relief
Stabilization Temperature 120°C – 175°C 120°C – 175°C
Stabilization Time 1–2 hours (typical) 3–5 hours (longer for thick plates)
Mg Content 4.0% – 4.9% 4.0% – 4.9%
Mn Content 0.4% – 1.0% 0.4% – 1.0%
Strain Hardening 15% – 25% 20% – 35%
Tensile Strength (MPa) 305 – 350 (thin plate) 310 – 370
Yield Strength (MPa, min) 215 240
Elongation (50mm, %) 10 – 12 8 – 10
Stress Corrosion Resistance Excellent (marine grade) Superior (military/armor grade)
High‑Temperature Strength Drops significantly above 110°C Maintains high strength at 120°C – 140°C
Typical Applications Ship structures, pressure vessels, chemical equipment Armor vehicles, ballistic plates, heavy naval structures
Hardness (HBW) 85 – 100 95 – 120
Exfoliation Corrosion (ASTM G44/G47) ≤ PB grade ≤ PB grade
Weldability Good Good (≥90% strength retention after welding)
Heat‑Treatable No No
  1. Key Terminology Corrections
Original Term Corrected Term Explanation
Softening temperature Stabilization temperature Standard term for stress‑relief annealing; no “softening temperature” in specs
Softening time Stabilization holding time Standard term for holding period during stabilization
Cold work rate Strain hardening level (cold work degree) Industry standard expression; H131 has higher strain hardening
h/mm (time unit) Hours (total holding time) Stabilization time is not per mm thickness; non‑standard unit removed
  1. Application Recommendations
  • Process parameters (temperature, holding time) are typical factory values, not mandatory standards. Label: “Typical parameters; subject to factory certification.”
  • Standard separation: H321 complies with EN/ASTM; H131 complies with ASTM/MIL. Avoid cross‑standard comparison.
  • For formal projects or customer documentation, use this revised version for consistent formatting and clear data.