sample of 5083H131 aluminum sheet with Inkjet coding

5083 H131 vs H116: What is the Difference for Shipbuilding?

Basic Information

Temper: H131

(Exclusive temper under ASTM/MIL standards, processed with special stabilization treatment. Excellent resistance to stress corrosion and exfoliation corrosion, non-heat treatable, exceptional weldability.)

Note: H131 temper is not defined in European Standard EN 485. Its equivalent high-performance marine-grade tempers are H116/H321.

Applicable Standards: EN 485, ASTM B209/B928, MIL-DTL-46027K (formerly MIL-A-46027)

Thickness Range: 0.5mm – 200mm (Full coverage for thin, medium and thick plates)

  1. Material Overview

5083 is an Al-Mg series high-magnesium corrosion-resistant aluminum alloy. The H131 temper is a specialized grade developed for naval vessels, armor and special load-bearing structures. It undergoes precise cold working and stabilization treatment, achieving an optimal balance between strength and corrosion resistance (especially exfoliation corrosion resistance). Boasting outstanding seawater/salt spray corrosion resistance, excellent low-temperature toughness and high post-weld strength retention, it is widely used in military armor, ship hulls, cryogenic pressure vessels and rail transit load-bearing components.

  1. Alloy Chemical Composition (wt%)

Slight variations exist across different standards. Detailed composition per standard is listed below for precise compliance.

Table 1: Chemical Composition per EN 573-3 / MIL-DTL-46027K (wt%)

Element Si Fe Cu Mn Mg Cr Zn Ti Single Others Total Others Al
Requirement ≤0.40 ≤0.40 ≤0.10 0.40–1.0 4.0–4.9 ≤0.25 ≤0.25 ≤0.15 ≤0.05 ≤0.15 Remainder

Table 2: Chemical Composition per ASTM B209 (wt%)

Element Si Fe Cu Mn Mg Cr Zn Ti Single Others Total Others Al
Requirement ≤0.40 ≤0.40 ≤0.10 0.40–1.0 4.0–4.9 0.05–0.25 ≤0.25 ≤0.15 ≤0.05 ≤0.15 Remainder

Key Element Functions

  • Mg: Primary strengthening element, enhances strength and corrosion resistance via solid solution strengthening.
  • Mn/Cr: Refine grain structure, inhibit intergranular corrosion and stress corrosion cracking, improve toughness of welded joints.
  1. Mechanical Properties

3.1 ASTM B928 / ASTM B209 (5083 H131)

Note: Standard data source for H131 temper. Only minimum values are specified for all properties.

Thickness (mm) Tensile Strength Rm (MPa, ≥) Yield Strength Rp0.2 (MPa, ≥) Elongation A50mm (%, ≥)
0.5–6.35 310 240 6
6.35–12.7 310 240 7
12.7–50 310 240 8
50–100 300 230 8
100–200 290 220 7

3.2 MIL-DTL-46027K (5083 H131, Armor Grade)

Note: Hardness is typically specified in purchase orders or reported as a reference value, with no broad range defined.

Thickness (mm) Tensile Strength Rm (MPa, ≥) Yield Strength Rp0.2 (MPa, ≥) Elongation A50mm (%, ≥) Hardness HBW
6.35–12.7 310 240 8 Reported or as agreed
12.7–25.4 310 240 9 Reported or as agreed
25.4–50.8 305 235 10 Reported or as agreed
50.8–76.2 300 230 10 Reported or as agreed

3.3 EN 485-2 (EN AW-5083) – Reference Equivalent Tempers

Note: H131 is not defined in EN standards. Equivalent high-strength, corrosion-resistant marine tempers H116/H321 are listed for parameter comparison.

Thickness (mm) Temper Tensile Strength Rm (MPa) Yield Strength Rp0.2 (MPa, ≥) Elongation A50mm (%, ≥)
0.5–6 H116/H321 305–380 215 6
6–12.5 H116/H321 305–380 215 7
12.5–40 H116/H321 305–380 215 8
40–80 H116/H321 295–370 200 8
80–200 H116/H321 285–360 190 7
  1. Supplementary Notes

The dimensional tolerance and key characteristics sections in the original document are accurate and can be retained as-is. This revision focuses on standardizing chemical composition table formatting, aligning Cr content across standards, clarifying mechanical property tempers, and standardizing military hardness specifications to ensure full compliance with authoritative standards and eliminate misleading information.