sample of 4045 aluminum sheet

4343 vs 4045 vs 4047 Aluminum‑Silicon Brazing Foils: Complete Technical Comparison

Introduction

Al‑Si brazing alloys are the backbone of modern aluminum joining technology. Among them, 4343, 4045, and 4047​ dominate global supply chains for heat exchangers, cooling systems, and lightweight structural assemblies. Their differences in silicon percentage directly influence melting point, fluidity, erosion tendency, and joint integrity—making correct selection essential for performance, reliability, and cost efficiency.

sample of 4045 aluminum sheet


1. Chemical Composition (wt%)

Element 4343 4045 4047
Silicon (Si) 6.8–8.2% 9.0–11.0% 11.0–13.0%
Iron (Fe) ≤0.80% ≤0.80% ≤0.80%
Copper (Cu) ≤0.25% ≤0.30% ≤0.30%
Manganese (Mn) ≤0.10% ≤0.05% ≤0.15%
Zinc (Zn) ≤0.20% ≤0.10% ≤0.20%
Aluminum (Al) Balance Balance Balance

2. Physical & Mechanical Properties (Annealed Condition)

Property 4343 4045 4047
Solidus / Liquidus 577–615°C 577–590°C 577–582°C
Freezing Range Wide (38°C) Medium (13°C) Very Narrow (5°C)
Density 2.68 g/cm³ 2.67 g/cm³ 2.66 g/cm³
Tensile Strength 100–160 MPa 120–180 MPa 140–200 MPa
Elongation ≥18% ≥15% ≥10%

3. Brazing Performance Comparison

Characteristic 4343 4045 4047
Flow & Gap Filling Moderate, controlled spread Balanced, stable flow Excellent capillary penetration
Base Metal Erosion Risk Lowest Medium Higher (requires precise temperature control)
Weld Leak Tightness Good Very Good Best (minimal defects)
Stamping / Formability Excellent (soft, ductile) Good Fair (higher hardness)
Process Window Wide tolerance Very wide tolerance Narrower tolerance

4. Typical Applications

  • 4343:​ Home AC evaporators/condensers, thin‑wall tubing joints, low‑cost general brazing, parts requiring deep stamping.
  • 4045:​ Automotive radiators, intercoolers, oil coolers, industrial plate‑fin exchangers—the mainstream choice for mass production.
  • 4047:​ High‑density plate‑fin exchangers, EV battery cooling plates, multi‑layer narrow‑gap assemblies, vacuum‑brazed high‑seal products.

5. Brazing Process Notes

  • All three alloys share a solidus of 577°C; typical brazing temperature range is 590–610°C.
  • For 4047, minimize soak time at peak temperature to prevent base metal erosion caused by rapid Si diffusion.
  • Keep foil surfaces clean and dry before assembly—oil, oxide, or moisture reduces wetting quality.
  • Post‑braze cleaning is mandatory after flux brazing to prevent corrosion from residual salts.

6. Quick Selection Guide

Requirement Recommended Grade
Thin walls, erosion‑sensitive parts, cost priority 4343
General‑purpose heat exchangers, stable mass production 4045
Complex geometry, micro‑gaps, strict leak‑tight specs 4047

Conclusion

Choosing between 4343, 4045, and 4047 comes down to balancing fluidity, erosion control, sealing performance, and manufacturability. 4343 is the safe, economical choice for thin‑walled assemblies. 4045 is the versatile workhorse for high‑volume production. 4047 is the premium solution for complex, high‑performance joints where nothing less than perfect sealing will do.